    ASC BRICK & CASTABLE FOR THE IRON LADLE

    LIFE > 1200 HEATS .

    It is mainly raw material made of electro-corundum (or sintered corundum, special glass bauxite clinker) and graphite and silicon carbide containing more than 90%-95% of fixed carbon.Add graphite, bauxite and additives, and make them by mixing, moulding, drying and firing at high temperature.

    Technical Parameters

    1、铝碳化硅碳砖 – ASC BRICK

    项     目 ITEM

    单位

    指标值

    体积密度 BD

    g/cm3

     ≥2.85

    常温耐压强度   CCS       

    Mpa

    ≥40

    高温抗折强度(1400℃×0.5h)MOR

    Mpa

    ≥5

     Al2O3

    %

    55-65

    C

    %

    5-12

    SiC

    %

    8-10

    2、铝碳化硅浇注料 – ASC CASTABLE (REPAIR CASTABLE )

    项    目 ITEM

    单位

    指标值

    Al2O3     

    %

    55-65

    SiC

    %

    6-10

    耐火度 REFRACTORINESS

    >1790    

    体积密度 BD

    g/cm3

     ≥2.6

    抗折强度

    MOR

    110℃×24h

    Mpa

    ≥6

    1500℃×3h

    Mpa

    ≥10

    耐压强度

    CCS

    110℃×24h

    Mpa

    ≥50

    1500℃×3h

    Mpa

    ≥80

    烧后线变化 PLC

    1500℃×3h

    %

    ±1